Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 58.7 J/cm | 110 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1614 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 58.7 J/cm | 110 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 6080 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 58.7 J/cm | 110 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1579 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |