Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 18 µm/km | 18 µm/km | |
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data) Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, .. |