Magnetic Properties | Metric | English | Comments |
---|---|---|---|
Core Loss | 4.41 W/kg @Magnetic Field 1.50 T, Frequency 60.0 Hz |
2.00 W/lb @Magnetic Field 1.50 T, Frequency 60.0 Hz |
0.025" (24 gauge); ASTM A677 |
AK Steel DI-MAX® M-19 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Core Loss | 4.41 W/kg @Magnetic Field 1.50 T, Frequency 60.0 Hz |
2.00 W/lb @Magnetic Field 1.50 T, Frequency 60.0 Hz |
0.0185" (26 gauge); ASTM A677 |
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Core Loss | 4.41 W/kg @Magnetic Field 1.50 T, Frequency 60.0 Hz |
2.00 W/lb @Magnetic Field 1.50 T, Frequency 60.0 Hz |
0.025" (24 gauge), Semi-Processed; ASTM A677 |
AK Steel DI-MAX® M-43 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |