Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | RWG, SRRG Powders |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | |
Epoxy Technology EPO-TEK® EK1000-MP Epoxy Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding .. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | |
Epoxy Technology EPO-TEK® H20E-MP Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-MP is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | |
Epoxy Technology EPO-TEK® H35-175MP Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H35-175MP is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-elec.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | |
Epoxy Technology EPO-TEK® H35-175MPLV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H35-175MPLV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-el.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | |
Epoxy Technology EPO-TEK® H35-175MPT Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H35MPT is a single component, silver-filled, electrically conductive epoxy designed for military hybrid die and component attach. High viscosity version of EPO-TEK® H.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | |
Epoxy Technology EPO-TEK® H37-MP Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H37-MP is a single component, electrically conductive, thixotropic silver-filled adhesive for die-attach and SMD attach inside hybrid microelectronic packages. Also av.. |
|||
Ionic Impurities - Na (Sodium) | <= 50 ppm | <= 50 ppm | |
Epoxy Technology EPO-TEK® H37-MPT Epoxy Material Description: A single component, silver-filled and electrically conductive adhesive designed for semiconductor die attach and bonding SMDs for hybrid microelectronic packaging. It is certi.. |