Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 1553 °C | 2827 °F | Ac3 |
Latrobe LSSâ„¢ D2 Tool Steel (ASTM D2) TLS D2 tool steel is a versatile high-carbon, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium rich alloy carbides.. |