Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 843 °C | 1550 °F | Ac1 |
Latrobe LSSâ„¢ H14 Tool Steel (ASTM H14) TLS H14 tool steel is a 5%-chromium hot work steel to which tungsten has been added for improved high-temperature properties and heat resistance. It is a deep-hardening, airhardening
steel that exh.. |
|||
Critical Temperature | 841 °C | 1550 °F | Ac1 |
Latrobe Starkâ„¢ ASTM M4 High Speed Steel STARK (M4) is a super high speed steel with very high carbon and vanadium contents for exceptional abrasion resistance. It is well suited for premium cutting tools of all types,
particularly those u.. |
|||
Critical Temperature | 846 °C | 1550 °F | Ac3 |
Latrobe CM-50â„¢ ASTM M50 High Speed Steel CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to.. |
|||
Critical Temperature | 843 °C | 1550 °F | |
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |