Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 774 °C | 1430 °F | Ar3 |
Latrobe TNWâ„¢ ASTM M10 High Speed Steel TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2%
vanadium content. TNW is popul.. |
|||
Critical Temperature | 774 °C | 1430 °F | Ar1 |
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1) TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load.. |
|||
Critical Temperature | 777 °C | 1430 °F | Ac1 |
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1) TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load.. |
|||
Critical Temperature | 777 °C | 1430 °F | Ar1 |
Latrobe Double Six™ ASTM M2 High Speed Steel DOUBLE SIX (M2) is a tungsten-molybdenum high speed steel with a well balanced composition suitable for a wide variety of applications. World wide, the M2 type is by far
the most popular high speed .. |
|||
Critical Temperature | 777 °C | 1430 °F | Ar3 |
Latrobe LSS™ H21 Hot Work Tool Steel (ASTM H21) TLS H21 hot work tool steel is a low-carbon, tungsten hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is intended for elevated-temperature service .. |