Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 729 °C | 1340 °F | Case Ac1 |
Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe.. |
|||
Critical Temperature | 729 °C | 1340 °F | Core Ac1 |
Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe.. |