Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 (Asia Pacific) LNP* Lubricomp* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific) LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific) LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |