Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.026 cm/cm @Time 86400 sec |
0.026 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.026 cm/cm @Time 86400 sec |
0.026 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 (Asia Pacific) LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.026 cm/cm @Time 86400 sec |
0.026 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |