Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0135 cm/cm @Time 86400 sec |
0.0135 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |