Polymer Property : Linear Mold Shrinkage, Flow = 0.0049 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0049 cm/cm

@Time 86400 sec
0.0049 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific)
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Linear Mold Shrinkage, Flow 0.0049 cm/cm

@Time 86400 sec
0.0049 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DFI12E PC
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Linear Mold Shrinkage, Flow 0.0049 cm/cm

@Time 86400 sec
0.0049 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer
LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0049 cm/cm

@Time 86400 sec
0.0049 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific)
LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber.