Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific) LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON PFD06 PA 6 LNP* STAT-KON* PFD06 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON PFD06 PA 6 (Asia Pacific) LNP* Stat-kon* PFD06 is a compound based on Nylon 6 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |