Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP JF006 PES LNP* THERMOCOMP* JF006 is a compound based on Polyethersulfone resin containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66 LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region... |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MV006SU PP LNP VERTON* MV006SU is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MV006SU PP (Asia Pacific) LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MV006SU PP (Europe-Africa-Middle East) LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MX02795 PP (Asia Pacific) LNP* Verton* MX02795 is a compound based on Polypropylene resin containing Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific) LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MX02795 PP LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural. |