Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect.. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized... |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 (Asia Pacific) LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC LNP THERMOCOMP* DF006ER is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11 LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0011 - 0.0016 cm/cm @Time 86400 sec |
0.0011 - 0.0016 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12 LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0011 - 0.0016 cm/cm @Time 86400 sec |
0.0011 - 0.0016 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific) LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0011 - 0.0016 cm/cm @Time 86400 sec |
0.0011 - 0.0016 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12 LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas .. |
|||
Linear Mold Shrinkage, Flow | 0.0011 - 0.0030 cm/cm @Time 86400 sec |
0.0011 - 0.0030 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6 LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Verton NV006E PC/ABS LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV006E PC/ABS (Asia Pacific) LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10 LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti.. |
|||
Linear Mold Shrinkage, Flow | 0.0011 cm/cm @Time 86400 sec |
0.0011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV006E PC+ABS LNP* Verton* NV006E is a compound based on PC+ABS blend resin containing 30% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |