Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA.. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0032 cm/cm @Time 86400 sec |
0.00060 - 0.0032 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0032 cm/cm @Time 86400 sec |
0.00060 - 0.0032 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific) LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0032 cm/cm @Time 86400 sec |
0.00060 - 0.0032 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0032 cm/cm @Time 86400 sec |
0.00060 - 0.0032 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0032 cm/cm @Time 86400 sec |
0.00060 - 0.0032 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific) LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0032 cm/cm @Time 86400 sec |
0.00060 - 0.0032 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0032 cm/cm @Time 86400 sec |
0.00060 - 0.0032 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |