Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Time 86400 sec |
0.0065 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Time 86400 sec |
0.0065 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC (Asia Pacific) LNP* Colorcomp* D1000P is a compound based on Polycarbonate resin containing Unfilled Custom Color. Added features of this material include: Exceptional Processing. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Time 86400 sec |
0.0065 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Time 86400 sec |
0.0065 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Time 86400 sec |
0.0065 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Time 86400 sec |
0.0065 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Time 86400 sec |
0.0065 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SU PP LNP* THERMOCOMP* MF006SU is a compound based on Polypropylene containing 30% lass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized. |