Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS LNP* LUBRICOMP* ZFG26 is a compound based on PPE+PS resin containing 30% Glass Fiber, 10% Graphite. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS (Asia Pacific) LNP* Lubricomp* ZFG26 is a compound based on PPE+PS Blend resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific) LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret.. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific) LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP 5C003 FP-V (PVDF) LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp 5C003 LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC.. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |