Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 LNP* THERMOCOMP* QF0069 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific) LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66 LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66 LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg.. |