Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.149 bar @Temperature 135 °C |
112 torr @Temperature 275 °F |
|
Dow Glycidyl Methacrylate Glycidyl Methacrylate For Aliphatic Epoxy Polymers (Clear, colorless liquid)Information provided by Dow |