Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 790 - 870 cSt @Temperature 25.0 °C |
790 - 870 cSt @Temperature 77.0 °F |
ASTM D445-94 |
Dow VORANOL™ CP 4711 Polyol VORANOL™ CP 4711 polyol is a medium reactivity, capped triol, polyether polyol especially designed for the production of molded flexible foam. It is normally used in all TDI or TDI/MDI blend formu.. |
|||
Viscosity Measure | 750 - 870 cSt @Temperature 25.0 °C |
750 - 870 cSt @Temperature 77.0 °F |
ASTM D445-94 |
Dow VORANOL™ CP 4702 Polyol VORANOL™ CP 4702 polyol is a high reactivity, capped triol, polyether polyol especially designed for the production of molded flexible foam. It is normally used in all TDI or TDI/MDI blend formula.. |