Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 1.1 cSt @Temperature 205 °C |
1.1 cSt @Temperature 401 °F |
ASTM D445 |
ExxonMobil Mobil Aero HFS Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Viscosity Measure | 1.1 cSt @Temperature 205 °C |
1.1 cSt @Temperature 401 °F |
ASTM D445 |
ExxonMobil Mobil Aero HFS Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |