Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.990 g/cc @Temperature 55.0 °C |
0.0358 lb/in³ @Temperature 131 °F |
|
BASF Pluracol® 2097 Molded Foam Polyol Description: Pluracol® 2097 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams, one-shot semi-flexible and microcellular foams. HR foams made with.. |
|||
Density | 0.992 g/cc @Temperature 70.0 °C |
0.0358 lb/in³ @Temperature 158 °F |
|
BASF Pluracol® 3042 Specialty Polyol Description: Pluracol® 3042 polyol is 41 hydroxyl number (nominal 4000 molecular weight) propoxylated polyether.Information provided by BASF |
|||
Density | 0.992 g/cc @Temperature 54.5 °C |
0.0358 lb/in³ @Temperature 130 °F |
|
BASF Pluracol® 816 Molded Foam Polyol Description: Pluracol® 816 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol .. |
|||
Density | 0.991 g/cc @Temperature 37.8 °C |
0.0358 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® P2010 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Density | 0.991 g/cc @Temperature 37.8 °C |
0.0358 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® P410R Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Density | 0.990 g/cc @Temperature 37.8 °C |
0.0358 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® P710R Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Density | 0.992 g/cc @Temperature 37.8 °C |
0.0358 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® 726 Specialty Polyol Description: Pluracol® 726 polyol is a 3000 molecular weight propylene oxide adduct of glycerine. Originally designed as a slabstock foam polyol, Pluracol 726 has found wide acceptance in specialty.. |
|||
Density | 0.992 g/cc @Temperature 54.4 °C |
0.0358 lb/in³ @Temperature 130 °F |
|
BASF Pluracol® 1421 Molded Foam Polyol Description: Pluracol® 1421 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol.. |