Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.991 g/cc @Temperature 37.8 °C |
0.0358 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® P2010 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Density | 0.991 g/cc @Temperature 37.8 °C |
0.0358 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® P410R Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |