Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.947 - 0.950 g/cc @Temperature 23.0 °C |
0.0342 - 0.0343 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT 11-285 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure pipes and connection elements for pipeline phase method. Application: Composition is intended to be processed into pressure pipes.. |
|||
Density | 0.947 - 0.950 g/cc @Temperature 23.0 °C |
0.0342 - 0.0343 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT 11-285D High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure pipes and connection elements for pipeline phase method. Application: Composition is intended to be processed into pressure pipes.. |