Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 344 g/l | 344 g/l | |
Dow Corning Z-2306 SILANE Dow Corning® Z-2306 Silane is high purity, undiluted isobutyltrimethoxysilane. When diluted with an appropriate solvent, it can be used in the formulation of water repellent products. Upon proper a.. |