Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 0.000 - 336 g/l | 0.000 - 336 g/l | Average value: 115 g/l Grade Count:13 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 - 33.0 g/l | 0.000 - 33.0 g/l | Average value: 5.50 g/l Grade Count:6 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 - 591 g/l | 0.000 - 591 g/l | Average value: 88.7 g/l Grade Count:7 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Aremco-Seal™ 613 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1150 ºF (620 ºC) |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Aremco-Seal™ 617 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC). |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabind™ 542 High Temperature Inorganic Binder Single part, low viscosity, water-dispersed, aluminum phosphate solution for penetrating ultra fine thermal spray applications to 3000°F (1650°C). |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 618-N High Temperature Ceramic Adhesive/Paste, Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 632 High Temperature Ceramic Adhesive/Paste, Mica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco HiE-Coat™ 840-C High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for ceramic fiber modules and refactories to 2500°F (1371°C) |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for dense refractories to 2500°F (1371°C) and stainless steel to 900°F (482°C) |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for carbon and stainless steel to 2000 °F (1093°C). |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled White paste used for bonding of Ceramic-to-Ceramic; Ceramic-Metal; and Quartz. Used in Heaters, Igniters, Resistors, Sensors. This one component system air dries in 1-2 hrs and is ready for use fol.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 g/l | 0.000 g/l | |
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Volatile Organic Compounds (VOC) Content | 0.000 - 766 g/l | 0.000 - 766 g/l | Average value: 173 g/l Grade Count:9 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |