Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Parker Chomerics CHO-BOND SV712 Conductive Epoxy CHO-BOND® 700 Series Adhesives for Microelectronics Packaging; these pure silver-filled epoxy pastes are designed to meet the demanding requirements of semiconductor and microelectronic packaging. .. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Parker Chomerics CHO-BOND 360-20 Conductive Epoxy Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Humiseal 1C55 Silicone Conformal Coating Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Humiseal 1C61 UV Cure Conformal Coating Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ 2400 Pipe Renewal Liner NSF/ANSI-61 certified polyurea formulation is 100% solids and contains no epoxy resin. It is designed to help solve a wide variety of problems common to potable water systems. It utilizes a trenchle.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ 80BG 536 Urethane Elastomer Scotchkote Urethane Elastomer 80BG 536 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components. Product Features:Properties simil.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ 80FG 532 Urethane Elastomer Scotchkote Urethane Elastomer 80FG 532 has been specifically developed as an elastomeric system with a high degree of flexibility for casting and molding rubber components.Product Features:Propertie.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ FP 812 External Wall Coating 3M Scotchkote External Wall Coating FP 812 has been specifically developed as a low maintenance, high build coating for cemetitious and plaster wall surfaces.Information provided by 3M |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ PR 415 Epoxy Concrete Repair Scotchkote Epoxy Concrete Repair PR 415 has been specifically developed as a three component 100% solids self priming concrete repair system.Product Features:Combines good application characteristic.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ 136 Encapsulation Coating Polynox Scotchkote Encapsulation Coating Polynox 136 is a water based acrylic anti corrosive coating specifically developed to provide long term protection and encapsulation of previously coated structures... |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ 162PWX Epoxy Coating 3M Scotchkote Epoxy Coating 162PWX is a 100% solid two-part epoxy coating that has been specifically developed for the long term protection of drinking water pipelines, storage and process tanks or .. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ 474 Epoxy Concrete Repair Scotchkote Epoxy Concrete Repair 474 has been specifically developed as a three component 100% solids high performance mortar for use as a heavy duty repair system for concrete surfaces.Product Feat.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
3M Scotchkote™ 60FG 534 Urethane Elastomer Scotchkote Urethane Elastomer 60FG 534 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components.Product Features:Physical properti.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, gray coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, white coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadi.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Volatile Organic Compounds (VOC) Content | 0.00 g/l | 0.00 g/l | |
Parker Chomerics CHO-BOND 1075 Silicone RTV Adhesive/Sealant Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposur.. |