Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond CleanerA Surface Cleaner Permabond Cleaner A is a general purpose industrial cleaner for cleaning and degreasing surfaces prior to bonding with any Permabond adhesive. Where surfaces are greasy or dirty, wiping with CLEANER.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET500 Epoxy Resin PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET536 Epoxy Resin PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH120 Anaerobic Threadlocker Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HL138 Anaerobic Retaining Compound Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM118 Anaerobic Threadlocker Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM161 Anaerobic Retaining Compound Permabond® HM161 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space’ between parts and upon cure unitiz.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH050P Pure Anaerobic Threadsealant PERMABOND® LH050 PURE anaerobic pipe sealant is single component paste that cures only when in contact with metal parts and oxygen is excluded. The sealant fills up the entire space between male an.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH054 Anaerobic Threadsealant Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with meta.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH197 Anaerobic Gasketmaker Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA4810 Toughened Acrylic Adhesive PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4810 has excellent adhesion to as received metal surfac.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV645 UV-curable Adhesive PERMABOND UV645 is a single part, fast curing, high viscosity UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV648 UV-curable Adhesive PERMABOND UV648 is a UV-curing adhesive developed for use on plastics. It has good adhesion to acrylic and contains a long-wavelength photo initiator to allow it to cure through UV-stabilized plasti.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV649 UV-curable Adhesive PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F804 Polyetheretherketone (PEEK) Liquid Dispersion VICOTE F804 has been specifically formulated to provide a resilient coating with high wear and abrasion resistance on ferrous substrates such as carbon and cast steels. These properties are retained.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F810 Grey Polyetheretherketone (PEEK) Liquid Dispersion The F810 Grey grades have been specifically formulated to provide a resilient coating with high wear and abrasion resistance combined with excellent release properties on ferrous substrates such as .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F816 Black Polyetheretherketone (PEEK) Liquid Dispersion VICOTE® is the brand name for the Victrex range of coatings. VICOTE Coatings are available through Victrex or its preferred coater network. The VICOTE F815 and F816Blk grades have been specificall.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond F201 Anaerobic Retainer Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH040 Anaerobic Retainer Permabond® HH040 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitiz.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond MM115 Anaerobic Threadlocker Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance... |
|||
Storage Temperature | 0.000 - 25.0 °C | 32.0 - 77.0 °F | |
Akzo Nobel Trigonox® C-C75 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates.Chemical Description: tert-Butyl peroxybenzoate, 75% solution in odorless mineral spiritsCAS Num.. |
|||
Storage Temperature | -20.0 - 25.0 °C | -4.00 - 77.0 °F | |
Akzo Nobel Trigonox® BPIC-C75 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates. Trigonox BPIC-C75 may also be used as an initiator for curing unsaturated polyester and vinyles.. |
|||
Storage Temperature | 10.0 - 25.0 °C | 50.0 - 77.0 °F | |
Akzo Nobel Trigonox® C Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, vinylacetate, acrylates and methacrylates. Trigonox C is a monofunctional peroxide which is used for the crosslinking of pol.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A1042 Anaerobic Threadlocker Permabond® A1042 is a rapid curing adhesive designed to lock and seal metal parts that subsequently may need to be dismantled for maintenance. The high vibration resistance makes Permabond A1042 pa.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM135 Anaerobic Retainer Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A1046 Anaerobic Retainer Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A118 Anaerobic Retainer Permabond® A118 is an anaerobic adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It exhibits high strength, ex.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A126 Anaerobic Retainer Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A136 Anaerobic Gasketmaker Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potent.. |