Storage Temperature 24.0 - 38.0 °C
75.2 - 100 °F
Dow PAPI™ 95 Polymeric MDI
PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethan..
Storage Temperature 24.0 - 41.0 °C
75.2 - 106 °F
Dow PAPI™ 20 Polymeric MDI
PAPI™ 20 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality value of 3.2 and high viscosity result in highly rigid foams. This product is design..
Storage Temperature 24.0 - 41.0 °C
75.2 - 106 °F
Dow PAPI™ 580 N Polymeric MDI
PAPI™ 580 N polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has high functionality (value of 3.0) and relatively high viscosity. Recommended for use in polyi..