Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | <= -20.0 °C | <= -4.00 °F | |
Akzo Nobel Trigonox® EHPS Polymerization Initiator Initiator for the (co)polymerization of styrene, acrylonitrile, vinylacetate, vinylchloride, vinylidenechloride, acrylates and methacrylates.Chemical Description: Di(2-ethylhexyl) peroxydicarbonate,.. |
|||
Storage Temperature | -20.0 - -15.0 °C | -4.00 - 5.00 °F | |
Akzo Nobel Trigonox® EHP-W40 Polymerization Initiator Initiator for the (co)polymerization of vinylchloride and vinylidenechloride.Chemical Description: Di(2-ethylhexyl) peroxydicarbonate, 40% emulsion in water and methanolCAS Number: 16111-62-9Acronym.. |
|||
Storage Temperature | -20.0 - -15.0 °C | -4.00 - 5.00 °F | |
Akzo Nobel Trigonox® EHP-W40S Polymerization Initiator Initiator for the (co)polymerization of vinylchloride and vinylidenechloride.Chemical Description: Di(2-ethylhexyl) peroxydicarbonate, flakes, 40% frozen emulsion in waterCAS Number: 16111-62-9Acron.. |
|||
Storage Temperature | -20.0 - -15.0 °C | -4.00 - 5.00 °F | |
Akzo Nobel Trigonox® EHP-W50 Polymerization Initiator Initiator for the (co)polymerization of vinylchloride and vinylidenechloride.Chemical Description: Di(2-ethylhexyl) peroxydicarbonate, 50% emulsion in water and methanolCAS Number: 16111-62-9Acronym.. |
|||
Storage Temperature | -20.0 - -15.0 °C | -4.00 - 5.00 °F | |
Akzo Nobel Trigonox® EHP-W60 Polymerization Initiator Initiator for the (co)polymerization of vinylchloride and vinylidenechloride.Chemical Description: Di(2-ethylhexyl) peroxydicarbonate, 60% emulsion in water and methanolCAS Number: 16111-62-9Acronym.. |
|||
Storage Temperature | <= -20.0 °C | <= -4.00 °F | |
Akzo Nobel Trigonox® SBP Polymerization Initiator Initiator for the (co)polymerization of ethylene, vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonateCAS Number: 19910-65-7Acronym: SBP; Tx SBPInformation provid.. |
|||
Storage Temperature | <= -20.0 °C | <= -4.00 °F | |
Akzo Nobel Trigonox® SBPS Polymerization Initiator Initiator for the (co)polymerization of vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonateCAS Number: 19910-65-7Acronym: SBP; Tx SBPInformation provided by Akzo.. |
|||
Storage Temperature | <= -20.0 °C | <= -4.00 °F | |
Akzo Nobel Trigonox® SBP-W50 Polymerization Initiator Initiator for the (co)polymerization of vinylchloride and vinylidenechlorideChemical Description: Di-sec-butyl peroxydicarbonate, 50% emulsion in water and methanolCAS Number: 19910-65-7Acronym: SBP.. |
|||
Storage Temperature | -20.0 - 25.0 °C | -4.00 - 77.0 °F | |
Akzo Nobel Trigonox® BPIC-C75 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates. Trigonox BPIC-C75 may also be used as an initiator for curing unsaturated polyester and vinyles.. |
|||
Storage Temperature | <= -20.0 °C | <= -4.00 °F | |
Akzo Nobel Trigonox® EHP Polymerization Initiator Initiator for the (co)polymerization of ethylene and vinylchloride.Chemical Description: Di(2-ethylhexyl) peroxydicarbonateCAS Number: 16111-62-9Acronym: EHP; OPP; Tx EHPInformation provided by Akzo.. |