Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.27 cP | 2.27 cP | |
Formosa Plastics Formolon® 676 PVC Homopolymer General Purpose Grade Resin F676 is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered .. |
|||
Relative Viscosity | 2.27 cP | 2.27 cP | |
Formosa Plastics Formolon® 676H PVC Homopolymer General Purpose Grade Resin F676H is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered.. |