Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 330 °C |
70 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT1141 PC XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 330 °C |
70 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT1141 PC (Asia Pacific) XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 330 °C |
70 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT1141 PC (Europe-Africa-Middle East) XHT1141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Index of Compound | 70 g/10 min @Load 5.00 kg, Temperature 265 °C |
70 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |