Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 41 g/10 min @Load 10.0 kg, Temperature 280 °C |
41 g/10 min @Load 22.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East) |
|||
Melt Index of Compound | 41 g/10 min @Load 2.16 kg, Temperature 265 °C |
41 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Melt Index of Compound | 41 g/10 min @Load 5.00 kg, Temperature 300 °C |
41 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Melt Index of Compound | 41 g/10 min @Load 5.00 kg, Temperature 300 °C |
41 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Asia Pacific) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Melt Index of Compound | 41 g/10 min @Load 5.00 kg, Temperature 300 °C |
41 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Melt Index of Compound | 41 g/10 min @Load 2.16 kg, Temperature 265 °C |
41 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Melt Index of Compound | 41 g/10 min @Load 2.16 kg, Temperature 265 °C |
41 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Melt Index of Compound | 41 g/10 min @Load 5.00 kg, Temperature 300 °C |
41 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Melt Index of Compound | 41 g/10 min @Load 5.00 kg, Temperature 300 °C |
41 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Europe-Africa-Middle East) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Melt Index of Compound | 41 g/10 min @Load 2.16 kg, Temperature 280 °C |
41 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East) Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Melt Index of Compound | 41 g/10 min @Load 2.16 kg, Temperature 280 °C |
41 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Melt Index of Compound | 41 g/10 min @Load 2.16 kg, Temperature 280 °C |
41 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Melt Index of Compound | 41 g/10 min @Load 2.16 kg, Temperature 280 °C |
41 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |