Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 22.5 g/10 min @Load 10.0 kg, Temperature 190 °C |
22.5 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® ENR 8556.00 Ethylene-Octene Copolymer Description: ENR 8556.00 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in extrusion applications such as tubing and profiles. This elastomer provides excellen.. |