Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 15 g/10 min @Load 3.80 kg, Temperature 280 °C |
15 g/10 min @Load 8.38 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Index of Compound | 15 g/10 min @Load 3.80 kg, Temperature 280 °C |
15 g/10 min @Load 8.38 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Index of Compound | 15 g/10 min @Load 3.80 kg, Temperature 280 °C |
15 g/10 min @Load 8.38 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 250 °C |
15 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 250 °C |
15 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Melt Index of Compound | 15 g/10 min @Load 2.16 kg, Temperature 265 °C |
15 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Melt Index of Compound | 15 g/10 min @Load 2.16 kg, Temperature 265 °C |
15 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Melt Index of Compound | 15 g/10 min @Load 2.16 kg, Temperature 250 °C |
15 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 265 °C |
15 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 250 °C |
15 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ASTM D1238 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 250 °C |
15 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Melt Index of Compound | 15 g/10 min @Load 1.20 kg, Temperature 280 °C |
15 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 31508/0003 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 31508/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. PVDF 31508/0003 also has a very low brittleness temperature, for.. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 32008/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 32008/0009 is an ultra-flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 32008/0009 also has a very low brittleness te.. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A .. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 32008/0003 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesExcellent low flame and low smoke pe.. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 31508/0009 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31508/0009 also has a very low brittleness temperatu.. |
|||
Melt Index of Compound | 15 g/10 min @Load 1.20 kg, Temperature 280 °C |
15 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Melt Index of Compound | 15 g/10 min @Load 1.20 kg, Temperature 280 °C |
15 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 31008/0003 Polyvinylidene Fluoride
(discontinued **) 3M™ Dyneon™ PVDF 31008/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31008/0003 also has a very low brittleness temperatu.. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 31008/0009 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesExcellent low flame and low smoke .. |
|||
Melt Index of Compound | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 32008/0000 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesInformation provided by Dyneon, A 3M.. |