Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 220 °C |
13 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ZLL12CP PC (Europe-Africa-Middle East) Medium viscosity general purpose flame retardant polycarbonate grade based on recycled material. Rated UL94 V2 at 1.5 mm. Limited color availability. |
|||
Melt Index of Compound | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ZLL12CP PC (Europe-Africa-Middle East) Medium viscosity general purpose flame retardant polycarbonate grade based on recycled material. Rated UL94 V2 at 1.5 mm. Limited color availability. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 260 °C |
13 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Honeywell Aegis™ HFX High Barrier Nylon
(discontinued **) Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is .. |
|||
Melt Index of Compound | 13 g/10 min @Load 10.0 kg, Temperature 200 °C |
13 g/10 min @Load 22.0 lb, Temperature 392 °F |
ASTM D1238 |
Kuraray HYBRAR® H7125 Hydrogenated Thermoplastic Rubber Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Melt Index of Compound | 13 g/10 min @Load 10.0 kg, Temperature 260 °C |
13 g/10 min @Load 22.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East) |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 280 °C |
13 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East) |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 340 °C |
13 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 340 °C |
13 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), .. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 265 °C |
13 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 265 °C |
13 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |
|||
Melt Index of Compound | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Melt Index of Compound | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Melt Index of Compound | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Melt Index of Compound | 13 g/10 min @Load 1.20 kg, Temperature 280 °C |
13 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East) VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |