Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Heatwave CF746 Polymer
(discontinued **) Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 .. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Vitiva PC715 PET
(discontinued **) Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 15041 PET
(discontinued **) Voridian polymer 15041 is a PET thermoplastic polyester.Applications/UsesCrystallized PET (CPET) trays |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 9921P PET Film
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 9921P PET Injection Molded
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman A12 PET
(discontinued **) Voridian Polymer A12 is currently produced to Eastman`s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer A12 is available i.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman CA12 PET
(discontinued **) Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman CB11E PET
(discontinued **) VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman CB12 PET
(discontinued **) Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman CM01 PET
(discontinued **) Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink c.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman GP800 PET
(discontinued **) Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman P76CC PET
(discontinued **) Voridian PET P76CC is used for dual ovenable containers and release paper.Applications/UsesDual ovenable containersRelease paper |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman PG400 PET
(discontinued **) Voridian PET PG400 is a general purpose resin is mostly supplied into Mexico and has a wide array of applications in container manufacturing.Applications/UsesBeverage packagingContainersFood packagi.. |
|||
Melt Density | 1.20 - 1.40 g/cc | 0.0434 - 0.0506 lb/in³ | DIN 53735 |
Stanelco Bioplast® Wrap 100 Biodegradable Plastic Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Aqua PJ002 PET Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer PJ.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Aqua PJ003 PET Voridian Aqua PET PJ003 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. This product is specifically designed f.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Eastobond 19411 Copolyester, Film Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Eastobond 19412 Copolyester, Film Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
DAK Americas Laser+® MB912 PET Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient pr.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 5214A PET
(discontinued **) Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe.. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |