Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Density | 1.09 g/cc | 0.0394 lb/in³ | Melt density |
Americas Styrenics Styron® 6010 High Impact Polystyrene
(discontinued **) STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac.. |
|||
Melt Density | 1.09 g/cc | 0.0394 lb/in³ | Melt density |
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro.. |