Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6060D Fiber Grade PLA NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech.. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6201D Fiber Grade PLA NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically .. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6202D Fiber Grade PLA NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically .. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6204D Fiber Grade PLA NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically .. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6251D Fiber Grade PLA NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv.. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6302D Fiber Grade PLA NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech.. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6751D Fiber Grade PLA NatureWorks® PLA polymer 6751D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6751D is designed for extrusion into mechanically .. |
|||
Melt Density | 1.08 - 1.12 g/cc @Temperature 230 °C |
0.0390 - 0.0405 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Melt Density | 1.08 g/cc @Temperature 285 °C |
0.0390 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Eastar 5445 PCTG Copolyester, Injection Molded
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Melt Density | 1.08 g/cc @Temperature 285 °C |
0.0390 lb/in³ @Temperature 545 °F |
ASTM D1238 |
Eastman Eastar 5445 PCTG Copolyester, Film
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co.. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6350D Fiber Grade PLA NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s.. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6400D Fiber Grade PLA NatureWorks® PLA polymer 6400D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6400D is designed for extrusion into mechanically .. |
|||
Melt Density | 1.08 g/cc @Temperature 230 °C |
0.0390 lb/in³ @Temperature 446 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f.. |
|||
Melt Density | 1.08 g/cc | 0.0390 lb/in³ | |
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Melt Density | 1.08 g/cc | 0.0390 lb/in³ | Melt density |
Styron Magnum™ 344HP ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Density | 1.08 g/cc | 0.0390 lb/in³ | Melt density |
Styron Magnum™ 357HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |