Physical Properties Metric English Comments
Carbon Dioxide Transmission 380 - 429 cc-mm/m²-24hr-atm
965 - 1090 cc-mil/100 in²-24hr-atm
Average value: 405 cc-mm/m²-24hr-atm Grade Count:4
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Carbon Dioxide Transmission 380 - 429 cc-mm/m²-24hr-atm
965 - 1090 cc-mil/100 in²-24hr-atm
Average value: 405 cc-mm/m²-24hr-atm Grade Count:3
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Carbon Dioxide Transmission 380 - 480 cc-mm/m²-24hr-atm
965 - 1220 cc-mil/100 in²-24hr-atm
Average value: 417 cc-mm/m²-24hr-atm Grade Count:12
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Carbon Dioxide Transmission 380 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
965 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
3800 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..
Carbon Dioxide Transmission 380 - 480 cc-mm/m²-24hr-atm
965 - 1220 cc-mil/100 in²-24hr-atm
Average value: 429 cc-mm/m²-24hr-atm Grade Count:20
Overview of materials for Polycarbonate, Molded