Physical Properties | Metric | English | Comments |
---|---|---|---|
Carbon Dioxide Transmission | 60.0 - 80.0 cc-mm/m²-24hr-atm | 152 - 203 cc-mil/100 in²-24hr-atm | 400µm; ASTM D1434 |
Stanelco Bioplast® GS 2189 Biodegradable Plastic Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i.. |