Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Moisture Vapor Transmission = 2.18 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.860 cc-mm/m²-24hr-atm
2.18 cc-mil/100 in²-24hr-atm
ASTM E96
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..
Moisture Vapor Transmission 0.860 cc-mm/m²-24hr-atm
2.18 cc-mil/100 in²-24hr-atm
Proc. E; ASTM E96
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 50 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal..