Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.360 - 0.750 cc-mm/m²-24hr-atm | 0.914 - 1.90 cc-mil/100 in²-24hr-atm | 40°C- 90% RH; based on 30 µm layer |
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Moisture Vapor Transmission | 0.360 - 0.750 cc-mm/m²-24hr-atm | 0.914 - 1.90 cc-mil/100 in²-24hr-atm | 40°C- 90% RH; based on 30 µm layer |
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo.. |