Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.960 - 1.74 cc-mm/m²-24hr-atm | 2.44 - 4.42 cc-mil/100 in²-24hr-atm | 40°C- 90% RH; based on 30 µm layer |
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Moisture Vapor Transmission | 0.960 cc-mm/m²-24hr-atm | 2.44 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 125 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack.. |