Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.820 cc-mm/m²-24hr-atm | 2.08 cc-mil/100 in²-24hr-atm | 40°C, 90% RH |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Moisture Vapor Transmission | 0.820 cc-mm/m²-24hr-atm | 2.08 cc-mil/100 in²-24hr-atm | 40°C, 90% RH |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |