Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.360 - 0.750 cc-mm/m²-24hr-atm | 0.914 - 1.90 cc-mil/100 in²-24hr-atm | 40°C- 90% RH; based on 30 µm layer |
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Moisture Vapor Transmission | 0.360 - 0.750 cc-mm/m²-24hr-atm | 0.914 - 1.90 cc-mil/100 in²-24hr-atm | 40°C- 90% RH; based on 30 µm layer |
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo.. |
|||
Moisture Vapor Transmission | 0.360 cc-mm/m²-24hr-atm | 0.914 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® AFG Polyolefin Shrink Packaging Film, Anti-fog, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially-oriented, heat-shrinkable, anti-fog polyolefin film. The film has excellent gloss, stretch recovery, toughness and tear resista.. |
|||
Moisture Vapor Transmission | 0.360 cc-mm/m²-24hr-atm | 0.914 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® RS900 Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, permeable antifog shrink film engineered for food packaging. It forms tight, leak-resistant heat seals. Printable grades (RST900) offer .. |
|||
Moisture Vapor Transmission | 0.360 cc-mm/m²-24hr-atm | 0.914 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Moisture Vapor Transmission | 0.360 cc-mm/m²-24hr-atm | 0.914 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Moisture Vapor Transmission | 0.360 cc-mm/m²-24hr-atm | 0.914 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Moisture Vapor Transmission | 0.360 cc-mm/m²-24hr-atm | 0.914 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Moisture Vapor Transmission | 0.360 cc-mm/m²-24hr-atm | 0.914 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Moisture Vapor Transmission | 0.360 - 3.10 cc-mm/m²-24hr-atm | 0.914 - 7.87 cc-mil/100 in²-24hr-atm | Average value: 1.13 cc-mm/m²-24hr-atm Grade Count:26 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Moisture Vapor Transmission | 0.360 cc-mm/m²-24hr-atm | 0.914 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |