Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.150 cc-mm/m²-24hr-atm | 0.381 cc-mil/100 in²-24hr-atm | ASTM D1434 |
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer. |
|||
Moisture Vapor Transmission | 0.150 cc-mm/m²-24hr-atm | 0.381 cc-mil/100 in²-24hr-atm | ASTM F1249 |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |