Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.0315 cc-mm/m²-24hr-atm | 0.0800 cc-mil/100 in²-24hr-atm | blown film sample; ASTM F1249-90 |
Dow XU 32046.31 Barrier Polymer Excellent oxygen and water vapor barrier Information provided by Dow |