Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.00606 - 0.354 cc-mm/m²-24hr-atm | 0.0154 - 0.900 cc-mil/100 in²-24hr-atm | Average value: 0.0960 cc-mm/m²-24hr-atm Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |